Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.24 GPa | 470 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Novablend™ 5035 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Tensile Modulus | 3.24 GPa | 469 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 3.24 GPa | 469 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP (Asia Pacific) LNP* THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 3.24 GPa | 469 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 3.24 GPa | 469 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 200-23 Polycarbonate Resin Overview: CALIBREâ„¢ 200-23 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 1mm/min; ASTM D638 |
Ensinger TECACRYL® TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to cr.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Ensinger TECAPET™ PET Polyethylene Terephthalate (PET) TECAPET™ PET is an unreinforced, semicrystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus,.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
CIP Composites 100 Series Laminated Polymer Bearing Material The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |