Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.85 GPa | 413 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Tensile Modulus | 2.85 GPa @Thickness 3.20 mm |
414 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Tensile Modulus | 2.85 GPa @Temperature 23.0 °C |
413 ksi @Temperature 73.4 °F |
|
LATI Latamid 66 MDT03-01 PA 66 Polyamide 66 (PA66) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® C CF 107 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Modulus | 2.85 GPa @Temperature 120 °C |
413 ksi @Temperature 248 °F |
1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 20YK270 PP SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl PKN4766 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4766 is a translucent PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulat.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | ISO 527 |
Polyram PlusTek PA340S05 Nylon 6.6 for Injection Molding, 5% Glass-beads Reinforced, Heat Stabilized 5% Glass-beads reinforced Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | ASTM D638 |
American Polymers API 375 Polystyrene API 375 is a general purpose polystyrene produced in pellet form for injection molding. API 375 has excellent strength and clarity as well as fast set-up properties.Applications: Used in the manufa.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | ISO 527 |
Polyram RamTough PZ303G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | ISO 527 - 1 & - 2 |
Asahi Kasei Tenac®-C 5520 Copolymer Acetal Resin Similar to TENAC®-C 4520 but with higher flow and minimized mold deposit.Information provided by Asahi Kasei Corporation. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Tensile Modulus | 2.85 GPa | 413 ksi | ISO 527 |
Radici Heraform® R 900 Acetal Copolymer Standard grade for injection molding of details with high mechanical requirement.Information provided by Radici group. |