Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.36 GPa | 342 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2710 TRN 9470 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXG121R PC PC in special effects colors. ""Diamond Sparkle"" appearance additives. Color package may affect performance. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXM123R PC (Europe-Africa-Middle East) FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXM123R PC FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | |
Ineos ABS Lustran® 488 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 POLYESTER ELASTOMER LNP* THERMOCOMP* YF005 is a compound based on Polyester Elastomer resin containing 25% Glass Fiber. |
|||
Tensile Modulus | 2.36 GPa | 342 ksi | 1 mm/min |
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No.. |
|||
Tensile Modulus | 2.36 GPa | 343 ksi | ASTM D638 |
Bayshore Vinyl Compounds BRC R7560 CLR 221 PVC Compound, Food Grade BRC R7560 CLR 221 is a food grade PVC bottle compound made with 100% FDA approved ingredients. This product exhibits excellent clarity and can be used in many applications where food contact is req.. |