Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.4 GPa | 1800 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PC-15CF-15GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinu Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | ASTM D638 |
LNP Lubricomp® UFL-4036 HS Polyphthalamide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | 5.0 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | ASTM D638 |
Applied Composites 8012 Polyester SMC Industry Application: SpecialtyProduct Application: Food EquipmentDistinct Features: NSF ApprovedInformation provided by Applied Composites Corporation. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | 1 mm/min |
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Tensile Modulus | 12.4 GPa @Treatment Temp. 70.0 °C, Time 180000 sec |
1800 ksi @Treatment Temp. 158 °F, Time 50.0 hour |
62% rel. humidity |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® RA-30CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | |
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 12.4 GPa | 1800 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AM 33 GF/000 L HS Black Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Heat StabilizedBlackEnhanced LubricationGlass Fiber ReinforcedInformation provided by PolyOne Corporation. |