Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir RK 451G Polystyrene UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded, high impact polystyrene. This grade combines medium flow, heat resistance and good light stability for injection moulding of technical p.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min |
Polimeri Europa KOBLEND HI PD 19 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with a very good impact behaviour, good stiffness and higher thermal properties than KOBLEND HI 18. Main application field.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min |
Polimeri Europa EDISTIR RC3 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-18 Special high impact, high gloss polystyrene grade. Suitable for injection molding in the appliances sector.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1mm/min |
Eastman Tenite 180A-28(HT) Cellulose Acetate
(discontinued **) 28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is develop.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
Styron INSPIREâ„¢ TF1500 ESU Polypropylene Talc filled, high impact PP compound. INSPIREâ„¢ TF1500 ESU has been developed for aesthetic automotive applications, with good scratch resistance and UV light stabilization.Information provided.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | ISO 527-2 |
Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion Daploy WB135HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | ASTM D638 |
Total PS CPDS 818 Easy Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 818 is a high heat resistant, high impact Polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacturing of articles which r.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | ASTM D 638 |
Cossa Polimeri ESTALUX 9206 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | ASTM D 638 |
Cossa Polimeri ESTALUX 9206 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
Tensile Modulus | 1.95 GPa | 283 ksi | ISO 527 |
Cossa Polimeri ESTABLEND PA 2500 ABS / Nylon 6 Blend ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri.. |