Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 0.120 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus >= 0.120 GPa
>= 17.4 ksi
MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.120 GPa
>= 17.4 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.120 GPa
>= 17.4 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.120 GPa
>= 17.4 ksi
2% sec, TD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.120 GPa
>= 17.4 ksi
2% sec, TD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.120 GPa
>= 17.4 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus 0.120 GPa
17.4 ksi
ISO 527-1/-2
Styrolution Styroflex® 2G 66 SBC
Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o..
Tensile Modulus 0.120 GPa
17.4 ksi
ISO 527-1/-2
DSM Arnitel® PM460-H TPC-ET
Injection Molding, Heat Stabilized
Tensile Modulus 0.120 GPa
17.4 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..