Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 500R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 915AU PC (Europe-Africa-Middle East) LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXM4701 PPC LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Americas .. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | ASTM D638 |
Covestro Apec® DP9-9340R High-Heat Polycarbonate, Medical with Release
(discontinued **) It is the responsibility of the medical device, biological product, or pharmaceutical manufacturer (Manufacturer) to determine the suitability of all component parts and raw materials, including the.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | 10%/min. ASTM D638 |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | (50mm/min); ISO 527-2/1A |
Aardvark Polymers AARTEL® 800 Rotational Molding Resin Aartel 800 is our high test, general purpose, acetal copolymer. Aartel 800 provides overall excellent performance for most applications and is available in natural (off white) and a wide range of st.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL TPN9221 PPE+PS (Asia Pacific) Transparent Noryl grade with 90dc and V-2 FR |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N850 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | ISO 527-1/-2 |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® 3158 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | ISO 527-1/-2 |
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 500SC NC010 Acetal (POM)
(Unverified Data**) Silicone Lubricated Medium Viscosity Acetal Homopolymer Concentrate Developed for Enhancing LubricityInformation provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers DIAMALOY PC 1008 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | ISO 527-1/-2 |
Covestro Makrolon® LQ3187 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable i.. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | ASTM D638 |
Solvay Specialty Polymers Mindel® S-1000 Modified Polysulfone
(discontinued **) This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001. |
|||
Tensile Strength, Yield | 66.0 MPa | 9570 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |