Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 38.6 MPa | 5600 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-PS-027-BA-WHT Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Tensile Strength, Yield | 38.6 MPa @Thickness 3.20 mm |
5600 psi @Thickness 0.126 in |
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 1402 C Clarified Polypropylene Homopolymer Thermoforming Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM D638 |
M. Holland Company PP510 Polypropylene Homopolymer AntistaticGood flowHomopolymerNucleatedGood stiffnessApplications: CapsClosuresDisposable hospital goodsHousehold goods |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM D638 |
Global MPP-120-C 20% Mica Reinforced Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | 2 in/min.; ASTM D638 |
Ineos H12Z-02 Polypropylene Homopolymer, Antistatic and Nucleated A nucleated and antistated polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications that require superior mold release pro.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® FRA205 ABS Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM-D638 |
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng.. |
|||
Tensile Strength, Yield | 38.6 MPa @Temperature 23.0 °C |
5600 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H35Z-00 Polypropylene Homopolymer This is a high flow rate, nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 C.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM D638 |
Techmer ES HiFill FR® ASA FR-2A WT209 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant, Good Toughness and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM D638 |
Techmer ES HiFill® PP GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: LubricatedInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM Data |
Styron Magnum™ 9043 ABS, High Gloss Sheet Extrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | Longitudinal |
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.002" thick) Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 4101N Staple Fiber and Injection Molding Polypropylene HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101N is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 4142T Injection Molding Polypropylene Homopolymer with Nucleating, Antistat AdditivesApplications: Appliance, closure and thin wall applications.Formolene 4142T is a low viscosity, highly isotactic polypropylene homopolymer designed pri.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 4143T Homopolymer Polypropylene Homopolymer for Injection Molded Applications Formolene® 4143T is a highly isotactic polypropylene for use in injection molded applications including cutlery and thin wall components. It contains a.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS VP-11 SHF Description: High Flow, Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | chs 0.2 in/min; ASTM D638 |
Diamond Polymers Centrex® 835 Sheet Extrusion Grade Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex .. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM D638 |
Clariant Renol PA2SP0004 Nylon 6 Alloy Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM D638 |
Clariant Renol SB83642580 ASA Polymer Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS VP-11 Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 38.6 MPa | 5600 psi | ASTM D638 |
Aclo Accutech Polypropylene HP0315V Homopolymer High Heat Approved to GMP.PP.013 |