Material Notes:
Homopolymer for Injection Molded Applications Formolene® 4143T is a highly isotactic polypropylene for use in injection molded applications including cutlery and thin wall components. It contains a unique combination of stabilizers and additives, which provides excellent processability and good end use performance. It has increased mold release for good handling of components. Formolene® 4143T meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min

@Temperature 230 °C
35 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 38.6 MPa
5600 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.65 GPa
240 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.374 J/cm

@Temperature 23.0 °C
0.700 ft-lb/in

@Temperature 73.4 °F
ASTM D256