Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
PolyMirae Moplen EP648N Injection Molding Grade Polypropylene Moplen EP648N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP648N is a high gloss block copolymer particularly suitable fo.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
PolyMirae Moplen HF600N Injection Molding Grade Polypropylene Moplen HF600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HF600N is a homopolymer with improved productivity and lower energy.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
PolyMirae Moplen HP526N IPP/WQBF Grade Polypropylene Moplen HP526N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP526N is a homopolymer particularly suitable for WQB (Water Quench.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
PolyMirae Moplen HP601N Injection Molding Grade Polypropylene Moplen HP601N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP601N is a homopolymer typically used by customers in Glass Mat Sh.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
PolyMirae Moplen HP602N Injection Molding Grade Polypropylene Moplen HP602N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP602N is a homopolymer particularly suitable for injection molding.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
PolyMirae Moplen HP640N Injection Molding Grade Polypropylene Moplen HP640N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640N is a homopolymer particularly suitable for injection molding.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
Hyosung Topilene S905 PP S905 Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
Hyosung Topilene S905H PP S905H Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 34.3 MPa @Thickness 3.20 mm |
4980 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Tensile Strength, Yield | 34.3 MPa @Thickness 3.20 mm |
4980 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Tensile Strength, Yield | 34.3 MPa @Thickness 3.20 mm |
4980 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL GP3300 PP+MF30% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 34.3 MPa @Thickness 3.20 mm |
4980 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
Global B-8200 High Density Polyethylene Description-high molecular weight, excellent stress cracking resistance,
excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC H1500 Polypropylene Homopolymer Features: SEETEC H1500 is a high flow homopolymer suitable for injection molding applications. SEETEC H1500 exhibits a high flowability combined with a good mechanical property balance. SEETEC H1500.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC H1501 Polypropylene Homopolymer Features: SEETEC H1501 is a homopolymer for injection molding. H1501 is specifically developed for application demanding a high stiffness and a high fluidity. SEETEC H1501 meets the FDA requirement .. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC H5300 Polypropylene, Homopolymer Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement .. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC H7411 Polypropylene, Homopolymer Features: Seetec H7411 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and U.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC H7500 Polypropylene, Homopolymer Features: Seetec H7500 is designed for the extrusion of continuous filament (CF). This grade is characterized by medium MWD and good processability from specific additives. SEETEC H7500 meets the FD.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC H7511 Polypropylene, Homopolymer Features: Seetec H7511 is designed for the extrusion of staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and UV stability. SEETEC H7511 mee.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC H7525 Polypropylene, Homopolymer Features: Seetec H7525 is designed for the extrusion of staple fibers. This grade is characterized by Medium MWD and good thermobonding, with anti-gas fading stabilization. SEETEC H7525 meets the FD.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC H7630 Polypropylene, Homopolymer Features: Seetec H7630 is designed for the extrusion of continuous filament (CF) & bulk continuous filament (BCF) fibers and staple fibers. This grade is characterized by medium MWD, with anti-gas f.. |
|||
Tensile Strength, Yield | 34.3 MPa @Thickness 3.20 mm |
4980 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical SH625 ABS, High Impact, High Flow Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIC 3704 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Medium Impact ResistanceUses: Rigid Packing; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ H5840B High Density Polyethylene Blow Molding Key Characteristics:Excellent environmental stress cracking resistance (ESCR)Excellent appearanceOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for food, juice, sof.. |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
Cheng Yu Plastic PE221 Flame Retardant LDPE |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
Cheng Yu Plastic PP226 Flame Retardant Polypropylene, Medium Impact |
|||
Tensile Strength, Yield | 34.3 MPa | 4980 psi | ASTM D638 |
Cheng Yu Plastic PP231H TALC 40 Polypropylene, 40% Talc, High Heat |
|||
Tensile Strength, Yield | 34.3 MPa @Thickness 3.20 mm |
4980 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL GP3100 PP+MF10% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |