Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 275 MPa @Strain 0.200 % |
39900 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4305 Austenitic Stainless Steel Good general corrosion resistance.Applications: Where machinability is required - threaded bar, studs, domestic appliances.Available in bar and rod forms. |
|||
Tensile Strength, Yield | 275 - 450 MPa @Strain 0.200 % |
39900 - 65300 psi @Strain 0.200 % |
|
Kobe Steel KS60 Commercially Pure Titanium, ASTM Gr. 2, Annealed Nominal Composition: Ti-Fe-OApplications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Relatively high strength, excellent corrosion resistance.. |
|||
Tensile Strength, Yield | 275 - 450 MPa | 39900 - 65300 psi | 0.2% proof |
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant... |
|||
Tensile Strength, Yield | 275 - 450 MPa | 39900 - 65300 psi | 0.2% proof |
Kobe Steel Titanium alloy with low alloying elements, ASTM Gr. 7, Annealed Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by .. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek HAYNES® 230 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK 23-35WCo Heat Resistant Stainless Steel Information provided by MetalTekCast ASTM A297 MOD. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK CE20N Cast UNS N08007 Austenitic Stainless Steel "300" series, general corrosion resistant alloyApplications: Nuclear, chemical and food processing. Valve and pump trim.Information provided by MetalTekCast UNS N08007; Cast Grade CE20N; Cast ASTM A.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK CW-12MW Cast UNS N30002 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK CW-2M Cast UNS N26455 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK N-12MV Cast UNS N30012 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek WC 6 Cast UNS J24054 Alloy Steel General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 540 °C |
39900 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 275 MPa @Temperature 870 °C |
39900 psi @Temperature 1600 °F |
|
Haynes Hastelloy® W alloy, gas tungsten arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK 617 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek WCC Cast 105-85 Alloy Steel General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 650 °C |
39900 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 540 °C |
39900 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Yield | 275 MPa | 39900 psi | Annealed |
Special Metals INCOLOY® Alloy 800 A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The.. |
|||
Tensile Strength, Yield | 275 MPa | 39900 psi | Annealed |
Special Metals NIMONIC® Alloy 75 A nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Used for sheet-metal fabrications in gas-turbine engines, for components of industrial furnace.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
ThyssenKrupp FR-30® Fire Resistant Steel With the newly developed FR 30 fire resistant structural steel from TKS there is now the possibility, for the first time, to create steel structures with a fire resistance rating up to F30 without a.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
AK Steel ASTM A 570, Grade 40 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
AK Steel ASTM A 907, Grade 40 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
AK Steel Formable, Grade 40K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) AK Steel Formable Grade - K indicates killed.Information provided by AK Steel |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 % |
39900 psi @Strain 0.200 % |
Typical; Annealed |
ATI Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100 AL 42 alloy is used extensively in the manufacture of sealed beam automobile head lamps, in grommet and pin type glass-metal seals, and in integrated circuit lead frames. It is also the core metal .. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
AK Steel ASTM A 1011, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 871 °C |
39900 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 230® alloy, GMAW deposit weld metal Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 538 °C |
39900 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |