Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Multibase Multi-Pro® 1008 T Polypropylene Talc Filler, 10% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 20-2501 C/AS Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Petromont 1201 High Density Polyethylene Resin Petromont HDPE 1201 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as multi-purpose shipp.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
ExxonMobil Escorene® HD-6704 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Toughness, Excellent Stiffness, Excellent ESCRUses: Industrial containers, Industrial lids |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Chevron Phillips HiD® 9330 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: base resin for use in utility and conduit pipe applicationsI.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2" (50mm) per min, Type IV; ASTM D638 |
Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE
(discontinued **) Extra High Molecular Weight Hexene Copolymer Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. Thes.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Ineos Nova Zyntar® 7000 Flame Retardant Polystyrene Features:General purpose workhorse resinGood flow for injection moldingUL94 V-0 @ 1.5 mm for all colors UL94 5VA rating FOAMED @ 4.6 mm, 0.87-1.07 g/cc density, natural colorCustom colors availableA.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Techmer ES HiFill FR® PP FR-N X BKN001 Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Plastics Group Polifil® RP-HDPE High Density Polyethylene Polifil® RP-High Density Polyethylene is a moderate stiffness material that retains excellent toughness. HDPE exhibits outstanding chemical resistance and environmental stress crack resistance. Inj.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 6510E Injection Molding Polypropylene Impact CopolymerApplications: General purpose injection molding of consumer products, household appliances, lawn and garden items and medical components.Formolene 6510E is a higher impact, medium st.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® E900 Pipe HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E900 is a high molecular weight high density polyethylene (HMW-HDPE) resin des.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2 in/min; ASTM D638 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Chevron Phillips Marlex® 9503HF High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP25-0116 Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Entec Hypro™ PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled Information provided by Entec |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Aclo Accucomp Polystyrene HS0600L High Impact |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 78A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Plastics Group Polifil® RP-HIPS High Impact Polystyrene Polifil® RP-High Impact Polystyrene (HIPS) combines the good stiffness properties of polystyrene, with enhanced impact properties gained by the addition of impact modifiers, usually butadiene rubbe.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Resirene Resirene® 7600 Super High Impact Polystyrene Features:Medium FlowSuper High ImpactEasy ProcessingHigh ProductivityFDA Rating: 21 CFR 177.1640Applications:InjectionToysCompounds and Master BatchPrintersComputersRemote ControlsInformation provid.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | >= 24.8 MPa | >= 3600 psi | ASTM D 638 type IV |
Total Finathene® 50100.3 HDPE blow molding
(discontinued **) Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging. Blow Molding Stock Temperature 370 – 450 ºF Extrusion melt tempera.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |