Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ISO 527 |
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ISO 527 |
Polimeri Europa Clearflex® RM 50 U Linear Medium Density Polyethylene Clearflex RM 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RM 50 U show good mecha.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 1880 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1880 engineered polyolefin is designed for large automotive applications that require dimensional stability over a broad temperature range. This material exhibits excellent pr.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | 50 mm/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 324-3561 LMDPE Rotational Molding Resin Description: ICORENE 324-3561 is a linear medium density polyethylene developed for use in rotational molding. It has very good flow properties allowing the material to reproduce fine detail and me.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ISO 527-1, -2 |
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
SPS Guang Zhou SAMATâ„¢ 5000C Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high impact, high heat resistance, meets the requirements of RoHs and PaHsApplications: E/E applianceInformation Provided by.. |
|||
Tensile Strength, Yield | 18.0 MPa @Temperature 80.0 °C |
2610 psi @Temperature 176 °F |
ISO Data |
Styrolution Luran® S 776 SE ASA Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between .. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | At 50 mm/min; ISO 527-2 |
Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion Borcoat EA165E is an elastomer modified compound, based on a high molecular weight copolymer. The elastomer modification gives excellent low temperature impact resistance.Borcoat EA165E is recommen.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | At 50 mm/min; ISO 527-2 |
Borealis Daplen™ EF040AE TPO Compound Daplen EF040AE is a elastomer modified polypropylene compound intended for injection molding. Daplen EF040AE is a material with excellent impact/stiffness ratio. Thanks to its low thermal expansio.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ISO 527 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIH 6007A Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Wire and Cable Applications Wire Types: V-90 Agency Ratings: AS 3147-1992 Forms: Pellets Processing Method: ExtrusionInformation Provided by.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ISO 527 |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | 2 in/min, Type IV bar; ASTM D-638 |
Chevron Phillips Marlex® C300 Polyethylene; Enhanced Metallocene medium density polyethylene. This metallocene MDPE resin is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typical blow molded ap.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | |
Covestro Bayflex® 110-50 Polyurethane Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ISO 527-2/B |
ExxonMobil Exxtral™ BMU 233 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact, good dimensional stability and good UV resistance.Availability.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | 50 mm/min |
Arkema Group Pebax® 5533 SN 70 NOIR Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Hardness 60 shore D Black antistatic grade Applications: Tube extrusion...ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 18.0 - 27.0 MPa | 2610 - 3920 psi | Spec; ISO 527-1/2 |
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost.. |
|||
Tensile Strength, Yield | 18.0 MPa @Strain 50.0 % |
2610 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Rilsan® BMV 400 TL Nylon 11 (Dry) Designation ISO 1874-PA11,M,18-002,ZFlexible grade for injection molding. Available color: natural. Light and heat stabilized. Plasticizing agent free.Outstanding impact strength and tear spreading .. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D-638 |
Bapolene® 3039U Polyethylene, Rotational Molding Grade Bapolene 3039U is a hexene linear low density polyethylene designed to provide superior impact resistance. It contains a UV-stabilization package and complies with US FDA 21CFR177.1520.Applications.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | 50 mm/min |
Polimeri Europa EDISTIR SRL550 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,E,083-12-07-18 High impact, easy flow polystyrene with good elasticity at low temperatures. Used for sheet extrusion and .. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
SCG Chemicals EL-Lene™ M50 Octene (C8) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tan.. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
LyondellBasell Astryn 73A6-3 Polypropylene Copolymer, 30% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, excellent aesthetics, high gloss, .. |
|||
Tensile Strength, Yield | 18.0 MPa | 2610 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |