Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® 5533 SN 70 NOIR Polyether Block Amide (PEBA) (Dry)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® 5533 SN 70 NOIR Polyether Block Amide (PEBA) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) Hardness 60 shore D Black antistatic grade Applications: Tube extrusion...ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Water Absorption 1.2 %
1.2 %
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength, Yield 18.0 MPa
2610 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 31 %
31 %
50 mm/min
Tensile Modulus 0.305 GPa
44.2 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched NB
NB
1.82 J/cm²

@Temperature -30.0 °C
8.66 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 159 °C
318 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.12e+7 ohm-cm
1.12e+7 ohm-cm
Surface Resistance 6.69e+6 ohm
6.69e+6 ohm