Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.2 MPa | 2500 psi | TM R050-36 |
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | at 100%; ASTM D412 |
1055D Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D 638 |
Styrolution PS 5410 HIPS Good printabilityGood environmental stress crack resistanceLow GelsTrims CleanlyLow Gloss (matte finish)Information provided by Styrolution |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D412 |
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
Techmer ES HiFill FR® PP CO FR-N Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
Total PSI 960E Polystyrene Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids .. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ISO 527-1/2 |
CTC X-PRO CTC PP 4025 Polypropylene Copolymer X-PRO PP 4025 is a high value polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ISO 527-1/2 |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ISO 527-1/2 |
CTC X-PRO PP 2050 Polypropylene Copolymer X-PRO PP 2050 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
ExxonMobil LL 6407.67 Injection Molding Resin L Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processa.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
ExxonMobil LLDPE LL 6407.67 Linear Low Density Polyethylene Resin Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processabi.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | 2.0 in/min; ASTM D638 |
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | 2.0 in/min; ASTM D638 |
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | 2.0 in/min; ASTM D638 |
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | 2.0 in/min; ASTM D638 |
ExxonMobil LLP8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D-638 |
Axiall 02540 Plenum Flexible PVC Non-lead stabilized Category 3 plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D-638 |
Axiall 1131-57D Wire & Cable Flexible PVC Non-lead stabilized 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D-638 |
Axiall 12880 Wire & Cable Flexible PVC 75C general purpose. 720 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D-638 |
Axiall 15880-02 Wire & Cable Flexible PVC TW, 60C oil. 80C Class 43 insulation. Oil resistant I. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D-638 |
Axiall 17883 Wire & Cable Flexible PVC UV resistant, 90C insulation compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D-638 |
Axiall 8780 Moldings & Extrusions Flexible PVC Low gravity, general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D-638 |
Axiall 8881 Moldings & Extrusions Flexible PVC Profile extrusion compound especially formulated to impart a matte surface appearance to the finished article.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D638 |
ExxonMobil LL 8555.67 Rotational Molding Resin
(discontinued **) LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir.. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | ASTM D-638 |
Axiall 22882 Coax & Telecom Flexible PVC Flexible flame retardant jacket compound suitable for "patch cable" constructions over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 17.2 MPa | 2500 psi | at 100%; ASTM D412 |
EG65D Polyurethane-based Biomedical Elastomer |