Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PSI 960E Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Total Atofina
Trade Name PSI
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSI 960E Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids and containers for salad dressings, gravies, and high fat dairy products. Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Elongation at Yield 65 %
65 %
ASTM D638
Tensile Modulus 1.59 GPa
230 ksi
ASTM D638
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm
2.90 ft-lb/in
ASTM D256
Falling Dart Impact 13.6 J
10.0 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 94.4 °C
202 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 98.3 °C
209 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 60 %
60 %
60°; ASTM D523