Axiall 15880-02 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 15880-02 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TW, 60C oil. 80C Class 43 insulation. Oil resistant I. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 91
85 - 91
delayed; ASTM D-2240
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Elongation at Yield 269.1 %
269.1 %
Air Aging: 7 days @ 113°C; 30 mil slabs; UL 1581
325 %
325 %
ASTM D-638
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 27 %
27 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F