Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
Nylene® PA6 Glass Filled 5213 HS Nylon 6 13% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Therma-Tech™ NJ-6000 TC Polyamide 12 (Nylon 12) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ISO 527, ASTM D638 |
Nilit Nilitop BT G4 FR C3 is a 20% Glass Fiber Reinforced, Flame Retardant PBT Description: Nilitop BT G4 FR C3 is a 20% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
Fiberfil® FPI-15 BK Nylon 6, 15% Glass Reinforced, post industrial Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 110 MPa @Strain 0.200 %, Temperature 982 °C |
16000 psi @Strain 0.200 %, Temperature 1800 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
Kostat 1940 Conductive PC Compound KOSTAT 1940 is a conductive thermoplastic compound based on Polycarbonate and a special carbon fiber. KOSTAT 1940 is not dependant on atmospheric conditions and is used for ESD injection molded pro.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1000M PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). UL94 V0, V2 and 5VA listing. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1100R PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM DU319 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
Techmer ES HiFill® PEI BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF13 FR 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
Techmer ES HiFill® TPX-HTN-01026 A 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM-D638 |
Polyram PlusTek PA320G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, flame retardant and high stiffness polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ISO 527-2 |
Tisan TISLAMID® 6 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM D638 |
Westlake Plastics Pomalux® 25% GF Acetal Copolymer 25% Glass Filled Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM-D638 |
Polyram RamSter RF300G4 PBT, 20% Glass Fiber 20% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | |
Chicago Extruded Metals UNS C38000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | |
Asahi Kasei Xyron® G703H Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Tensile Strength, Yield | 110 MPa | 16000 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |