Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Mixed 1:2; TM R050-36 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | ASTM D412 |
Precision Polymer Engineering N65E Nitrile Rubber Nitrile Butadiene Rubber (NBR) 62-72 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5509 Grade C (inactive for new de.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | 50% Elongation; ASTM D412 |
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Tensile Strength, Yield | 6.89 - 13.8 MPa | 1000 - 2000 psi | ASTM D1708 |
Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | Insulating Layer |
Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | Insulating Layer |
Fujipoly Industries Zebra® 1002 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | Support Rubber |
Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | Support Rubber |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | Insulating Layer |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | Support Rubber |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | Insulating Layer |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | Insulating Layer |
Fujipoly Industries Zebra® 2004 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
Tensile Strength, Yield | >= 6.89 MPa @Strain 300 % |
>= 1000 psi @Strain 300 % |
|
Sibur SKD 1st Grade Butadiene Rubber (BR) BR 1220. It is used in tires and the rubber and asbestos technical industries. Rubbers produced on a base of butadiene rubber are extremely resistant to wearing. |
|||
Tensile Strength, Yield | >= 6.89 MPa @Strain 300 % |
>= 1000 psi @Strain 300 % |
|
Sibur SKD Superior Quality Butadiene Rubber (BR) BR 1220. It is used in tires and the rubber and asbestos technical industries. Rubbers produced on a base of butadiene rubber are extremely resistant to wearing. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3301-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex APEX® 3310-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2760 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2840E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2890M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | |
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | |
Trelleborg E602 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | cured 72 hrs @ RT |
ACC QM 270 QSI Quantum Silicones 70 Durometer Addition Cure Moldmaking Material QM 270 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |
|||
Tensile Strength, Yield | >= 6.89 MPa | >= 1000 psi | ASTM D638 |
Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | 6.90 MPa | 1000 psi | |
ACC QM270 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: expanded PU foam, large obje.. |
|||
Tensile Strength, Yield | 6.89 MPa @Strain 300 % |
1000 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1537 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 6.89 MPa @Strain 300 % |
1000 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3985 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | TM R050-36 |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |