Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors

Category Polymer , Thermoset , Silicone
Manufacturer Fujipoly Industries
Trade Name Zebra®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carbon Zebra Connector is grater than the contact pad density of either LCD or PCB. At least one conductive layer will connect when the two mating surfaces are aligned and compressed. The insulation layer will insure isolation from adjacent circuits.Information provided by Fujipoly Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 10
10
Support Sponge
25
25
Support Rubber
55
55
Insulating Layer
73
73
Conductive Layer
Tensile Strength, Yield 2.90 MPa
421 psi
Support Sponge
5.90 MPa
856 psi
Conductive Layer
6.90 MPa
1000 psi
Support Rubber
6.90 MPa
1000 psi
Insulating Layer
Elongation at Yield 100 %
100 %
Support Sponge
100 %
100 %
Conductive Layer
250 %
250 %
Support Rubber
250 %
250 %
Insulating Layer
Tear Strength 5.00 kN/m
28.5 pli
Support Sponge
7.00 kN/m
39.9 pli
Conductive Layer
10.0 kN/m
57.1 pli
Support Rubber
10.0 kN/m
57.1 pli
Insulating Layer
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 5.0 ohm-cm
5.0 ohm-cm
Conductive Layer
1.00e+14 ohm-cm
1.00e+14 ohm-cm
Support Sponge
1.00e+14 ohm-cm
1.00e+14 ohm-cm
Support Rubber
1.00e+14 ohm-cm
1.00e+14 ohm-cm
Insulating Layer
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Between Layers
Descriptive Properties Value Comments
Color Black
Conductive Layer
Light Blue
Support Rubber
Off-White
Insulating Layer
Pink
Support Sponge
Continuity Resistance 1000 ohms
Current Carrying Capacity 50 mA
0.90mm by 0.90mm Pad