| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | TM R050-36 |
| Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
| Tensile Strength, Yield | 6.90 MPa | 1000 psi | ASTM D412 |
| Precision Polymer Engineering N65E Nitrile Rubber Nitrile Butadiene Rubber (NBR) 62-72 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5509 Grade C (inactive for new de.. |
|||
| Tensile Strength, Yield | 6.89 - 13.8 MPa | 1000 - 2000 psi | ASTM D1708 |
| Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
| Tensile Strength, Yield | 6.90 MPa | 1000 psi | Support Rubber |
| Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
| Tensile Strength, Yield | 6.90 MPa | 1000 psi | Insulating Layer |
| Fujipoly Industries Zebra® 1002 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
| Tensile Strength, Yield | 6.90 MPa | 1000 psi | Insulating Layer |
| Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
| Tensile Strength, Yield | 6.90 MPa | 1000 psi | Support Rubber |
| Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
| Tensile Strength, Yield | 6.90 MPa | 1000 psi | Support Rubber |
| Fujipoly Industries Zebra® 2004 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | Elastic; ASTM D412 |
| Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
| Tensile Strength, Yield | >= 6.89 MPa @Strain 300 % |
>= 1000 psi @Strain 300 % |
|
| Sibur SKD 1st Grade Butadiene Rubber (BR) BR 1220. It is used in tires and the rubber and asbestos technical industries. Rubbers produced on a base of butadiene rubber are extremely resistant to wearing. |
|||
| Tensile Strength, Yield | >= 6.89 MPa @Strain 300 % |
>= 1000 psi @Strain 300 % |
|
| Sibur SKD Superior Quality Butadiene Rubber (BR) BR 1220. It is used in tires and the rubber and asbestos technical industries. Rubbers produced on a base of butadiene rubber are extremely resistant to wearing. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412-97 |
| Saint-Gobain Norprene® A-60-F Food Process Tubing Formulation Description: Norprene® Food Process Tubing, Formulation A-60-F: Formulated to withstand the high temperatures frequently occurring during food and beverage processing, Norprene® Food Process.. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412-98 |
| Saint-Gobain Norprene® A-60-G Industrial Grade Tubing Formulation Description: Norprene® Industrial Grade Tubing, Formulation A-60-G: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and appl.. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | 100%; ASTM D412 |
| Teknor Apex APEX® 3302-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
| Teknor Apex MONPRENE® MP 2840E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
| Teknor Apex MONPRENE® MP 2890M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | Longitudinal |
| Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.010" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
| Teknor Apex TEKBOND® 6000-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
| Teknor Apex TEKBOND® 6700-65 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
| A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
| A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | |
| Tra-Con Tra-Bond 9392 Flexible Potting Epoxy Adhesive TRA-BOND 9392 is a low viscosity, two-part polyurethane formulation recommended for potting and molding where flexibility and temperature resistance are required. TRA-BOND 9349 is a room temperature.. |
|||
| Tensile Strength, Yield | 6.90 MPa | 1000 psi | |
| Trelleborg E602 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
| Tensile Strength, Yield | 6.90 MPa | 1000 psi | cured 72 hrs @ RT |
| ACC QM 270 QSI Quantum Silicones 70 Durometer Addition Cure Moldmaking Material QM 270 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
| Teknor Apex APEX® 1700-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met.. |
|||
| Tensile Strength, Yield | 6.89 MPa @Strain 300 % |
1000 psi @Strain 300 % |
ASTM D412 |
| Teknor Apex Monprene® MP 1537 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
| Tensile Strength, Yield | 6.90 MPa @Strain 50.0 % |
1000 psi @Strain 50.0 % |
50 mm/min |
| Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
| Tensile Strength, Yield | 6.89 - 20.7 MPa | 1000 - 3000 psi | Average value: 16.5 MPa Grade Count:5 |
| Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
| PolyOne Synprene® IT 38-082 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerOver-Molding GradeTransparentMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided b.. |
|||
| Tensile Strength, Yield | 6.89 MPa | 1000 psi | TM R050-36 |
| Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |
|||