Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
Custom Resins Vexel™ 5100 RD PBT; 15% Glass Filled
(discontinued **) Improved Surface. Property data for dry as molded samples.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC LNP* Lubricomp* Lexan_LF1520A compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12 LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HTX1010F PEI (Asia Pacific) Higher impact, Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific) LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6 LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
Entec Hypro™ PPH-GF30 Natural Homopolymer Polypropylene, 30% Glass Reinforced Information provided by Entec |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food .. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | 5 mm/min; ISO 527 |
Eurostar Starflam PX06011 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06011 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin (also known as Starflam PF1005Z222)Information provided by Eurosta.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | 5 mm/min; ISO 527 |
Eurostar Starflam PX08029 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX08029 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 93.0 MPa @Temperature -40.0 °C |
13500 psi @Temperature -40.0 °F |
ISO Data |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced High impact Nylon 66 reinforced with 13% glass fibers.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |