Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 41.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid)
Caution: To be used as an additive only.Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy..
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ DP 4980-1-1000 Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Strength, Yield 41.4 MPa
6000 psi
51 mm/min; ASTM D638
PolyOne Trilliant™ HC X THC 1101 Natural Copolyester
Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri..
Tensile Strength, Yield 41.4 MPa
6000 psi
5.1 mm/min; ASTM D638
PolyOne Edgetek® X TR2-10TA/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa..
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ SF M7000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 51 mm/min; ASTM D638
PolyOne Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Tensile Strength, Yield 41.4 MPa
6000 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® FRA203 ABS
Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech CamAlloy /ABS Weatherable Sheet
Description: Weatherable SheetInformation provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech Korad® SP-9011 Cap ABS Sheet
Description: ABS SheetInformation provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Star Plastics ABS3030 Molding Grade ABS
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Star Plastics ABS405 Extrusion Grade ABS
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Star Plastics ABS9020 Molding Grade ABS
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES HiFill® PP GF10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES Plastiblend® ABS/PBT 1000
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D 638
Styrolution PS 2610 GPPS
Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM Data
Styron Magnumâ„¢ 1040 ABS, Very High impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Clariant Renol BR4014BK ABS, High Gloss, Black
Data provided by Clariant Masterbatches
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall UV-6670 Rigid PVC, Molding
Georgia Gulf UV-6670 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Bapolan® 6055 Polystyrene, Injection Molding
Bapolan PS6055 is a crystal polystyrene resin designed for injection molding applications requiring fast cycle times and superior optical properties. It complies with US FDA21 CFR177.1640 and 94HB ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall UV-7160 Rigid PVC, Molding
Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Asahi Kasei Thermylene® F6-10FG-0100 10% Glass Fiber Reinforced, Chemically Coupled
Information provided by Asahi Thermofil
Tensile Strength, Yield 41.4 - 127 MPa
6000 - 18400 psi
Average value: 62.7 MPa Grade Count:37
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Oxford Polymers H-Acetal 20PTFE 20% PTFE Reinforced Homopolymer Acetal  (discontinued **)
20% PTFE Reinforced Homopolymer AcetalInformation provided by Oxford Polymers.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall 5055 Rigid PVC, Extrusion, Natural
Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p..
Copyright © lookpolymers.com All Rights Reserved