Polymer Property : Tensile Strength, Yield = 250 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 250 MPa
36300 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)  (Unverified Data**)
Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f..
Tensile Strength, Yield 250 MPa

@Strain 0.200 %,
Temperature 870 °C
36300 psi

@Strain 0.200 %,
Temperature 1600 °F
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 250 MPa

@Temperature 870 °C
36300 psi

@Temperature 1600 °F
Haynes Hastelloy® W alloy, shielded metal arc welds, as-welded
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 250 MPa

@Strain 0.200 %,
Temperature 870 °C
36300 psi

@Strain 0.200 %,
Temperature 1600 °F
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 250 MPa

@Strain 0.200 %,
Temperature 870 °C
36300 psi

@Strain 0.200 %,
Temperature 1600 °F
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 250 MPa
36300 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber
Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla..
Tensile Strength, Yield 250 MPa

@Strain 0.200 %
36300 psi

@Strain 0.200 %
Annealed prior to test
Special Metals BRIGHTRAY® Alloy 35 Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 1920°F (1050°C). It is similar to BRIGHTRAY alloy F but with rare-earth additions for greater resist..
Tensile Strength, Yield 250 MPa
36300 psi
Annealed
Special Metals INCOLOY® Alloy 800HT™
A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo..
Tensile Strength, Yield 250 MPa

@Strain 0.200 %
36300 psi

@Strain 0.200 %
Annealed prior to test
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â..
Tensile Strength, Yield 250 - 320 MPa

@Strain 0.200 %
36300 - 46400 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 400DP High-strength Steel
High-strength SteelComments: Docol DP - Cold Rolled Steel - dual-phase steel. Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact composition is..
Tensile Strength, Yield 250 MPa
36300 psi
ISO 527
Polyram Polytron A60N01 Nylon 6.6, 60% Long Fiber Glass
60% Long fiber glass reinforced natural Nylon 6.6, heat stabilized, for injection molding.Information provided by Polyram.
Tensile Strength, Yield 250 - 350 MPa

@Strain 0.200 %
36300 - 50800 psi

@Strain 0.200 %
CLAL-MSX NICLAL 3444 H12 1/2 Hard Copper Alloy, Free Cutting Bronze
Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b..
Tensile Strength, Yield 250 MPa
36300 psi
ASTM D638
E-Polymers TEKAMID® TB120G60W , 62% Glass Fiber Reinforced PA6, DAM
High strength, weather resistanceInformation provided by E-Polymers Co. Ltd.
Tensile Strength, Yield >= 250 MPa
>= 36300 psi
AK Steel ASTM A 570, Grade 36 Hot Rolled Carbon Steel, Structural Quality (SQ)
For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p..
Tensile Strength, Yield 250 MPa

@Temperature 700 °C
36300 psi

@Temperature 1290 °F
R<sub>p</sub>02
Assab Steels HOTVAR Hot Work Steel
HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue..
Tensile Strength, Yield 250 MPa
36300 psi
Typical
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, 1149°C (2100°F) Solution Treated, UNS N06601
Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increa..
Tensile Strength, Yield >= 250 MPa
>= 36300 psi
AK Steel ASTM A 1011, Grade 36 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Tensile Strength, Yield >= 250 MPa
>= 36300 psi
AK Steel ASTM A 1011, Grade 36 Type 2 Hot Rolled Carbon Steel, Structural Steel (SS)
Type 2 for conversion to A36Information provided by AK Steel
Tensile Strength, Yield >= 250 MPa
>= 36300 psi
AK Steel ASTM A 568 and A 635 Hot Rolled Carbon Steel, Structural Steel (SS)
For conversion to A36 plateInformation provided by AK Steel
Tensile Strength, Yield >= 250 MPa
>= 36300 psi
AK Steel ASTM A 907, Grade 36 Hot Rolled Carbon Steel, Structural Quality (SQ)
For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p..
Tensile Strength, Yield 250 MPa
36300 psi
As Cast
AFE Technologies Cronite 37Ni/18Cr/Nb No. HR32
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..
Tensile Strength, Yield 250 MPa

@Strain 0.200 %
36300 psi

@Strain 0.200 %
Typical after Solution Annealing
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants
Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum..