Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.0 MPa | 3190 psi | 2in (50mm) per min.; ASTM D638 Type 4 |
Polymer Industries Densetec HDPE Pipe Grade The material displays improved performance characteristics in a variety of piping applications. In addition the material is UV stabilized and ideal for use in demanding outdoor applications. It reta.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 Type IV |
Chevron Phillips Marlex® C579 High density polyethylene
(discontinued **) Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceApplications: multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containersInformation pro.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 Type IV |
Chevron Phillips Marlex® HHM TR-480Z/M362 Natural high density ethylene hexene copolymer/black concrete
(disc Benefits: good long term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures, concrete base resinCharacteristics: Pipe Ring ESCR > 2000 h, ASTM F 1248;.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman M2004-P Polyethylene
(discontinued **) M2004-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M2004-P has been found to exhibit good barrier properties, temperature res.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | 50 mm/min; ASTM D638 |
NOVA Chemicals Sclair® 2607-UV14 HDPE Injection Molding Resin Excellent stiffness, Good impact resistance, Low warpageApplications: Roll-out cartsAdditives: Elevated levels of ultraviolet stabilizer packages, Elevated levels of antioxidantsInformation provided.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ISO 527 |
Fiberfil® PP-60/TC/15/VO/ND Polypropylene Homopolymer, 15% Talc Filled, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer Features: Excellent stiffness and low temperature ductility.Applications: Injection Molding: Automotive interior energy management solutionsInformation Provided by Flint Hills Resources |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | GB1040 |
JPJ Technologies HDPE Pipe Grade Information provided by JPJ Technologies |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
Lucent Polymers TPO-30T Thermoplastic Polyolefin, 30% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
LyondellBasell Adsylâ„¢ 5C30F Thermoplastic Olefin Resin Primary Processing Method: Film extrusionKey Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature,.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
LyondellBasell Astryn 75A6-2 Polypropylene Copolymer, 20% Calcium Carbonate Key Features: conventional melt flow, medium modulus, mineral-filled polypropylene copolymer, high impact, excellent chemical resistance, excellent aesthetics, high gloss, good colorability, good pr.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
LyondellBasell Hifaxâ„¢ ETA-5081 Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convoluted .. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili.. |
|||
Tensile Strength, Yield | 22.0 - 28.0 MPa | 3190 - 4060 psi | ASTM D638 |
Solvay Specialty Polymers solvene® 250 EAP Electroactive Polymer (EAP) Annealing Temperature - < 135 °C; Breakdown Voltage - 250 kV/mm; Coercive Field - 50 kV/mm; Crystallization Point - ASTM D3418 123 °C; Curie Temperature - ASTM D3418 110 °C; d33 - -38.0 pC/.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | Crosshead speed 100 mm/min; ISO 527 |
SCG Chemicals EL-Leneâ„¢ H5211PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA, LNE, AENOR,.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | At 50 mm/min; ISO 527-2 |
Borealis Borstar® MB7541 High Density Polyethylene for Injection Molding Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D 638 |
Cossa Polimeri ESTASTIR HI 0412 Polystyrene Polystyrene for injection molding or extrusionHigh impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | parallel; ISO 527-3 |
Covestro Desmopan® DP 1960AW Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
Braskem CP 241 Injection Molding Polypropylene Description: CP 241 is a high melt flow rate heterophasic copolymer used for general purposes. This product offers excellent processability, easy mould filling, productivity as well as good stiffnes.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436W10L Wollastonite Reinforced |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436M10L Mica Reinforced |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436M40L Mica Reinforced |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | |
Addcomp PRIEX® 25095 Maleic Anhydride Grafted PP random copolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
ExxonMobil Escorene® HD-8761 HDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Tensile Strength, Yield | 22.0 MPa @Strain 0.200 %, Temperature 899 °C |
3190 psi @Strain 0.200 %, Temperature 1650 °F |
0.059" Coil |
AK Steel 15 Cr-Cb® ULTRA FORM® Ferritic Stainless steel AK Steel’s 15 Cr-Cb ULTRA FORM® is a low-carbon, low-nitrogen ferritic grade of stainless steel with an intermediate, 14.5% chromium content. Alloying additions of Ti, Cb, Si and Mn provide excell.. |
|||
Tensile Strength, Yield | 22.0 MPa @Temperature 100 °C |
3190 psi @Temperature 212 °F |
ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
Reliance Industries Relene C31101 Polyethylene Steel pipe coating High Density Polyethylene grade. Contains a minimum 2% of well dispersed carbon black.Characteristics:excellent weathering resistance, excellent processability, excellent adhesio.. |