Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 190 MPa | 27600 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Trilliant™ HC HC6620-0033 RS Natural Polyamide 66 (Nylon 66) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Oxford Polymers Oxnilon 66-43GF 43% Glass Fiber Filled Nylon 66 for Injection Molding 43% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ISO 527, ASTM D638 |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ASTM D638 |
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 316 °C |
27600 psi @Strain 0.200 %, Temperature 601 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 870 °C |
27600 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 556® alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanica.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF HS UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcements, 33% Filler by WeightAdditive: Lubricant, Heat Stabilizer and UV Stabilizer Features: Lubricated, Good UV Re.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 550 °C |
27600 psi @Strain 0.200 %, Temperature 1020 °F |
Solution Annealed prior to test |
Special Metals INCONEL® Alloy G-3 A nickel-chromium-iron alloy with additions of molybdenum and copper. It has good weldability and resistance to intergranular corrosion in the welded condition. The low carbon content helps preven.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: LubricatedTPCI# 8682101Information provided by TP Composite.. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 L UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceTPCI# 82.. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RF007S PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF007S is a compound based on PA 66 resin containing Glass Fiber . Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph.. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ISO 527 |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ASTM D638 |
PlastxWorld Veroplas PB3400 Nylon 66 general purpose, 40% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ASTM-D638 |
Polyram PlusTek PA301G7 Nylon 6.6, Heat Stabilized 35% Glass Fiber Heat stabilized 35% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ASTM-D638 |
Polyram PlusTek PA303G33 Nylon 6.6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ASTM-D638 |
Polyram PlusTek PA303G43 Nylon 6.6, 43% Glass Fiber 43% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ISO 527 |
Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction 30% Glass fiber reinforced Nylon 66 for low friction applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ASTM-D638 |
Polyram PlusTek PB300G7 Nylon 6, 35% Glass Fiber 35% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | 5 mm/min; ISO 527 |
Eurostar Staramide RF007S PA66, 35% Glass Fiber Filled, Injection Molded Staramide RF007S is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ASTM D638 |
E-Polymers TEKAMID® TA210G33 , 33% Glass Fiber Reinforced PA66, DAM 33% Glass Fiber reinforced, High strengthInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 190 MPa | 27500 psi | ASTM D638 |
Asahi Kasei Thermylon® NSG-440A-H 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, Conditioned Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | |
Ametek Ultra 304L P/M Stainless Steel, Sintered from 6.2 g/cc Green Density Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i.. |
|||
Tensile Strength, Yield | 190 MPa | 27600 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Tensile Strength, Yield | >= 190 MPa | >= 27600 psi | Minimum Guaranteed |
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 649 °C |
27600 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes Hastelloy® N, 1.14 mm sheet, heat treated at 1149°C (2100°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |