Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 152 MPa | 22000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 604 35 HS Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | |
Osprey Metals CE17M Al-Si Controlled Expansion Alloy Al-27%Si+ controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RH Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced Information provided by Ravago. |
|||
Tensile Strength, Yield | 152 - 230 MPa | 22000 - 33400 psi | Average value: 183 MPa Grade Count:6 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Yield | 152 MPa @Thickness 3.20 mm |
22000 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID HI2302A(W) PA6+GF30%, High Impact Feature: Injection Molding, PA6+GF30%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | .01% permanent set |
Meehanite GA-50 Flake Graphite Cast Iron Type GA-50 combines high strength, toughness, wear resistance and damping capacity with excellent machinability. Responds well to heat treatment, local and surface hardening.General Meehanite infor.. |
|||
Tensile Strength, Yield | 152 MPa @Thickness 3.20 mm |
22000 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific) LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
Tensile Strength, Yield | 152 MPa | 22100 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF33 IM2 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF33 IM L NAT001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedAppearance.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 C10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightFeatures: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF/M40 ML2 GY 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and He.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 CF10 TS15 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(13%) and Silicone Lubricant(2%)Features: Lubricated Appearance: BlackInforma.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6 GF40 IM HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 IM1 HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedAppearance: BlackInformation.. |
|||
Tensile Strength, Yield | 152 - 359 MPa | 22000 - 52000 psi | 0.2% offset |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | Offset not specified |
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Ashley Polymers Ashlene® PE126 PET Polyester, 30% Glass Reinforced PET Polyester, with 30% glass reinforcement.Data provided by the manufacturer |