Osprey Metals CE17M Al-Si Controlled Expansion Alloy

Category Metal , Nonferrous Metal , Aluminum Alloy
Manufacturer Osprey Metals, Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Osprey Metals CE17M Al-Si Controlled Expansion Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Al-27%Si+ controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 220 MPa
31900 psi
Tensile Strength, Yield 152 MPa
22000 psi
Thermal Properties Metric English Comments
CTE, linear 15.3 µm/m-°C

@Temperature 25.0 - 100 °C
8.50 µin/in-°F

@Temperature 77.0 - 212 °F
16.8 µm/m-°C

@Temperature 25.0 - 500 °C
9.33 µin/in-°F

@Temperature 77.0 - 932 °F
17.0 µm/m-°C

@Temperature 25.0 - 200 °C
9.44 µin/in-°F

@Temperature 77.0 - 392 °F
17.7 µm/m-°C

@Temperature 25.0 - 300 °C
9.83 µin/in-°F

@Temperature 77.0 - 572 °F
Specific Heat Capacity 0.7673 J/g-°C
0.1834 BTU/lb-°F
Thermal Conductivity 146.5 W/m-K

@Temperature 200 °C
1017 BTU-in/hr-ft²-°F

@Temperature 392 °F
146.8 W/m-K

@Temperature 25.0 °C
1019 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Component Elements Properties Metric English Comments
Aluminum, Al 73 %
73 %
Silicon, Si 27 %
27 %