Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 15.0 MPa | >= 2180 psi | ISO 527 |
Murtfeldt Material ”S”® 1000 Green Polyethylene Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
Okulen® 1000 PE-UHMW, Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527 |
Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene Flexirene MR 56 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | -25% change after 70 hours @ 150°C; ASTM D412 |
Precision Polymer Engineering Z85T Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 80-90 °IRHD. Medium acrylonitrile content (ACN =36%). ASTM D2000 line call-out M2DH920, A26, B16, EO16, EO36, F14, Z1, where Z1 = Hardness 80-90.Appli.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | |
LyondellBasell Lupolen® 3220 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | |
LyondellBasell Lupolen® 3226 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-1, -2 |
LyondellBasell Hifaxâ„¢ CB251 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB251 medium melt flow, 1,200 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of impact resis.. |
|||
Tensile Strength, Yield | 15.0 - 18.0 MPa @Thickness 2.00 mm |
2180 - 2610 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific) LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SSH 6009 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Flexibility Uses: Cable Jacketing; Wire and Cable Applications Wire Types: ST1; ST2; Type 9; Class 1/3; YM3; YM5 Agency Ratings: BS 6746; IEC 60502; JIS 672.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D638 |
Trelleborg Horda Cable E8560 Strippable Semiconductive Shielding E8560 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8560 meets the requirements as bel.. |
|||
Tensile Strength, Yield | 15.0 MPa @Strain 100 % |
2180 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 3055D Polyurethane injection molding gradewith high mechanical strength for articles subject to wearexcellent abrasion resistancegood wear resistancevery short cycle timesApplicationInjection molded engineering partsR.. |
|||
Tensile Strength, Yield | 15.0 MPa @Strain 300 % |
2180 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8785 A Polyurethane injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-1/-2 |
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ H1025 Performance Polyolefin Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.Availability.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-1/2 |
CTC SunPro® SP 200 TF 3033 Polypropylene Copolymer, 33% Talc Filled SunPro® SP 200 TF 3033 is a 33% talc filled polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Application: VW TL 52660 MD 03Data .. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-1/-2 |
DSM Arnitel® UM552 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | 50 mm/min |
Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided .. |
|||
Tensile Strength, Yield | 15.0 - 25.0 MPa | 2180 - 3630 psi | Spec; ISO 527-1/2 |
Axion Polymers Axpoly® PS01 3003 Enhanced White General Purpose Polystyrene PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437C20L1 Calcium Reinforced |
|||
Tensile Strength, Yield | 15.0 MPa @Strain 50.0 % |
2180 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength.. |
|||
Tensile Strength, Yield | 15.0 MPa @Temperature 80.0 °C |
2180 psi @Temperature 176 °F |
ASTM Test |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D-638 |
Axiall 163 Moldings & Extrusions Flexible PVC 60°C rated, high flow, electrical molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR DBPH-50 MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | 2 in/min; ASTM D638 |
Solvay Engineered Polymers DEXFLEX® 880 TPO
(discontinued **) Description: DEXFLEX® 880 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, good processabil.. |
|||
Tensile Strength, Yield | 15.0 - 41.4 MPa | 2180 - 6000 psi | Average value: 29.8 MPa Grade Count:13 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Tensile Strength, Yield | 15.0 - 46.9 MPa | 2180 - 6800 psi | Average value: 31.3 MPa Grade Count:14 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM-D638 |
Polyram RamOfin PPC371B50 Polypropylene, 50% Mineral Filled 50% mineral filled, heavy density polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |