Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 124 MPa | 18000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GMF 600 A 40 HS Natural Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | |
Pacific Sintered Materials F-241-S Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-15All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 124 MPa @Strain 0.200 % |
18000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys MIM-2200 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PK-10GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NL-20GF/000 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF25 IM L 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill FR® PA4/6 GF30 FR HS X 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant and Heat StabilizedUL File Number: E.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF25 FR HS L 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF20 L BK002 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Additive: LubricantFeatures: Lubricated and High FlowAppearance: BlackTPCI# 8376102Info.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF/M38 HS BK 38% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 38% Filler by Weight and Mineral Filler, 38% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabili.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF20 TL10 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: PTFE Lubricant (10%)Features: LubricatedAppearance: Natural ColorInformation p.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PEEK GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PPS GF/M65 BK 65% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 65% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES Luriblend® PA11 GF30 TL20 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Good Wear Resistance, Low Extractables, Lubricat.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF006P PC LNP THERMOCOMP* DF006P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill FR® PA4/6 GF30 FR HS X 30% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant and Heat StabilizedUL File Number: E.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D-882 |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2919 Fluoropolymer Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Tensile Strength, Yield | 124 MPa @Strain 0.200 % |
18000 psi @Strain 0.200 % |
|
Universal Wire Works 4043 (AMS 4190) Aluminum Alloy Filler Metal Alloy 4043 is a 5% silicon aluminum alloy designed to weld many similar and dissimilar cast and wrought aluminum parts. This alloy is excellent for types 4043, 6063, 5052, 6061, 355, 356 and others... |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | |
Vista Metals ATP-5™ Precision Cast Aluminum Plate Used where flatness and dimensional control are critical, such as: computer & electronics, pharmaceuticals, medical testing equipment, packaging machinery, printing machinery, thermoforming tools, m.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | |
Vista Metals Duramold-5™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |
|||
Tensile Strength, Yield | 124 - 221 MPa | 18000 - 32000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, Annealed Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Engineered Polymer Solutions PET 5300 FR, 30% Glass Filled Natural and colors available. Injection molding grade. Uses: General Purpose, pump housings, electricalInformation provided by Engineered Polymer Solutions. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Clariant Renol 6608G33HSL Nylon 66, 33% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | |
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ PI-05CF/000 EM Polyetherimide (PEI)