Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
Polimeri Europa Riblene® MP 31 Low Density Polyethylene - Injection Molding Riblene MP 31 is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 are characterized by a medium rigidity.Main Applications: Riblene MP 31 i.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
Polimeri Europa Riblene® MR 30 Low Density Polyethylene - Injection Molding Riblene MR 30 is a high fluidity low density polyethylene resin (LDPE) characterized by a high flowability and a medium rigidity.Parts made with Riblene MR 30 are characterized by good mechanical an.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D412 |
Precision Polymer Engineering R70D Natural Rubber Natural Rubber, 65-75 °IRHD. Formulated to Defence Standard 93-30, Type QX, Grade 70 (NRQX70).Applications: Natural rubber offers low compression set, high tensile strength, high resilience and ex.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D412 |
Precision Polymer Engineering V70H Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administ.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D412 |
Precision Polymer Engineering V72H Fluoroelastomer Compound Fluoroelastomer Rubber, 65-75 °IRHD. FDA grade. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admi.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | -25% change after 70 hours @ 150°C; ASTM D412 |
Precision Polymer Engineering Z80B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 75-80 °IRHD. Medium acrylonitrile content (ACN = 33.5%). ASTM designation = HNBR. ASTM D2000 line call-out 4MDH716, A26, B36, EO16, EO36, F14, Z1. Z1 .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D 638 |
NOVA Chemicals Novapol® LM-0724-A LDPE Injection Molding Resin LM-0724-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 500 mm/min; ASTM D638 |
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Strength, Yield | 12.0 - 307 MPa | 1740 - 44500 psi | Average value: 154 MPa Grade Count:81 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | |
Chevron Phillips 7105T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 50% Elongation; ASTM D412 |
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding
(discontinued **) Low density radical polyethylene made by high pressure process. Temperature profile (°C) for injection molding: 200 to 260Information provided provided by Total Petrochemicals.Total Petrochemicals .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA (Asia Pacific) LNP* THERMOCOMP* UX05504 is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | At 50 mm/min; ISO 527-2 |
Borealis Bormed™ LE6607-PH LDPE for Pharmaceutical Blow Molding Bormed LE6607-PH is a LD-polyethylene produced in a high pressure process intended for blow molding of sot and flexible packages for pharmaceutical products.Bormed LE6607-PH can be used in "blow-fil.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | MD/TD; ISO 527-3 |
Borealis FG5224 Linear Low Density Polyethylene FG5224 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-block and medium slip additives. This grade is developed for production of lamination film. FG5224 .. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM-D638 |
Polyram RamOfin PPC371B73 Polypropylene, 73% Mineral Filled 73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 50 mm/min |
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 2 in/min, Type IV bar; ASTM D638 |
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRBroad fusion rangeExcellent melt strengthGood processabilityExcellent flexibilityImproved output and texturingApplications: Coextruded ca.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 50.0 % |
1740 psi @Strain 50.0 % |
|
Covestro Texin® 985 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer Mater.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | 50 mm/min |
Arkema Group Pebax® 5533 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE(PEBA) hardness 55 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: overmolded parts for sport good (Footba.. |
|||
Tensile Strength, Yield | 12.0 MPa @Temperature 120 °C |
1740 psi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Tensile Strength, Yield | 12.0 MPa @Temperature 120 °C |
1740 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM-D638 |
Braskem ML2400N LLDPE Injection Molding Polyethylene The resin ML2400N is a linear low-density polyethylene, 1-butene based, with good flexibility and low warpage. It does not contain a slip agent. It does have narrow molecular weight distribution. Th.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Huntsman PE2051 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Very good molding processability, produces parts with good stiffness, and shows excellent flatness in large projected areas. Also recommended for multi-cavit.. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Huntsman PE2072 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, gloss, and stiffness.Applications: Injection molding: lids and difficult to fill applications... |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | |
BASF Novolen® 2900 NC Polypropylene Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 12.0 MPa | 1740 psi | ASTM D638 |
Huntsman PE2062 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High flow characteristics combined with good glossApplications: Injection molding: large moldings including housewares and toys.FDA Notes: Conforms to FDA reg.. |
|||
Tensile Strength, Yield | 12.0 - 67.0 MPa | 1740 - 9720 psi | Average value: 37.9 MPa Grade Count:7 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |