Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ISO 527-3
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene
Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
SABIC 218B Linear Low Density Polyethylene for Cast Film
Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ISO 527-3
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Film Tensile Strength at Break, MD 31.0 MPa

@Thickness 0.400 mm
4500 psi

@Thickness 0.0157 in
ISO 527
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend
The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend
The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
SABIC HP0322N Low Density Polyethylene for Blown Film
Product Description: HP0322N is a Low Density Polyethylene grade suitable for producing heavy duty films and contains no slip or antiblock additives. It yields outstanding toughness and optical pr..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Eastman E6838-902F Polyethylene Film  (discontinued **)
Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business ..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Eastman E6838-964F Polyethylene  (discontinued **)
E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
ExxonMobil LD 135.09 Cast Packaging Film Resin  (discontinued **)
LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Braskem PB 525/64 LDPE Blown Film Extrusion Polyethylene  (discontinued **)
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Automatic packaging of liquids products (FFS). Information provided by Braskem
Film Tensile Strength at Break, MD 31.0 - 41.4 MPa
4500 - 6000 psi
ASTM D882
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
MD-TD Average; ASTM D882
DuPont Elvax® 3165SB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ISO 527-3
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer
Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Westlake Elevate™ EF563 6.5% Ethylene Vinyl Acetate Copolymer
Westlake EF 563 resin is a fractional melt index 6.5% EVA copolymer with excellent drawdown, low melting/dispersion, and clarity optics in a soft but very tough film. Kosher compliant.Application/U..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
ExxonMobil Escorene® LD 713.93 Blown Film Resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhibits very high impact strength, high clarity, and excellent heat sealability.Availability: Lat..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin
Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade)
Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No..
Film Tensile Strength at Break, MD 31.0 MPa

@Thickness 0.0250 mm
4500 psi

@Thickness 0.000984 in
ASTM D882
Equate EFDC-7050 LLDPE Film Extrusion Resin
EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Huntsman PE1061 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film
The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc..
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolym..