ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend PartnerConstruction FilmFoamsHeavy Duty BagsHigh Performance Collation ShrinkPallet Shrink FilmProfile ExtrusionInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ExxonMobil method
Melt Flow 0.33 g/10 min
0.33 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
Film Elongation at Break, MD 160 %
160 %
ASTM D882
Film Elongation at Break, TD 650 %
650 %
ASTM D882
Puncture Energy 2.15 J
1.58 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 120 g
120 g
ASTM D1922
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
Dart Drop Test 170 g
0.375 lb
ASTM D1709A
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Film Tensile Strength at Break, TD 26.9 MPa
3900 psi
ASTM D882
1% Secant Modulus, MD 221 MPa
32000 psi
ASTM D882
1% Secant Modulus, TD 296 MPa
43000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 233 °C
<= 451 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 16 %
16 %
ASTM D1003
Gloss 38 %
38 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 17 lbf
ExxonMobil Method