DuPont Elvax® 3165SB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3165SB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent drawability for easy processing, good flex-crack resistance for liquid packaging, high toughness, low shrink for water bath applications, and excellent optical properties. It adheres to many materials. It is commonly used as a tie layer in certain coextrusions with dissimilar surfaces.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Moisture Vapor Transmission 1.42 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
3.61 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
g-mm/m²-day; based on film thickness; ASTM E96; ASTM E96
Oxygen Transmission 264 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
671 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
film; ASTM D3985
Melt Flow 0.70 g/10 min
0.70 g/10 min
Condition not noted.; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 530 %
530 %
MD-TD Average; ASTM D882
Film Elongation at Break, TD 530 %
530 %
MD-TD Average; ASTM D882
Impact 31.6
31.6
J/mm Spencer Impact; Average of MD and TD; ASTM D3420
Elmendorf Tear Strength, MD 4.17 g/micron
106 g/mil
Average of MD and TD; ASTM D1922
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
MD-TD Average; ASTM D882
Thermal Properties Metric English Comments
Melting Point 68.0 °C
154 °F
Freezing Point via DSC/ASTM D3418
88.0 °C
190 °F
Freezing Point via DSC/ASTM D3418
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 28 %
28 %
ASTM D1003
Gloss 40 %
40 %
20°; ASTM D2457