Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
SABIC 218 Series Linear Low Density Polyethylene for Blown Film Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Reliance Industries Reclair F22020 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Reclair F22020 has optimum levels of antioxidants, antiblocking agents, and slip additives. Applications:general purpose, and.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882-02 |
Ipiranga Petrochem LB 0120 BPS LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882-02 |
Ipiranga Petrochem LBH 0120 BPS LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene LDPE 2100TN00: Heavy duty film suitable for application in shrink hoods, industrial sacks, heavy duty carrier bags and liners.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene LDPE 2004TC37: Light duty film used for very thin films requiring good optical properties for general packaging.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene 235F7 is a LLDPE blown film grade designed for general purpose film application. This resin is particularly suited for blending with LDPE, giving better strength and downgauging possibility.Informat.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527 |
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene LS0085/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: shrink packaging.Information prov.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | |
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2070D Polyethylene resin is a fully formulated linear low density polyethylene resin offering high strength and low gel properties for blown film food packaging applications. DOWLEX 2070D r.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | |
Dow LDPE 494A Low Density Polyethylene, Film Grade DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | >= 12.0 MPa | >= 1740 psi | |
Iran Petrochemical (PCC) Tabriz 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 12.0 - 30.0 MPa | 1740 - 4350 psi | Average value: 24.2 MPa Grade Count:5 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Westlake Hifor SC74560-F Clear Polyethylene
(discontinued **) Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck.. |