Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Flexirene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an optimum balance between mechanical properties (stiffness) and sealing properties.Main Applications: Flexirene FG 30 is recommended for the production of general purpose film, automatic packaging and food packaging, especially when food is submitted to continuous cooking.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.925 g/cc
0.925 g/cc
ISO 1183
Thickness 15.0 - 50.0 microns
0.591 - 1.97 mil
Recommended
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527-3
Film Tensile Strength at Yield, TD 13.0 MPa
1890 psi
ISO 527-3
Film Elongation at Break, MD 600 %
600 %
ISO 527-3
Film Elongation at Break, TD 800 %
800 %
ISO 527-3
Coefficient of Friction, Dynamic >= 0.50
>= 0.50
ISO 8295
Elmendorf Tear Strength, MD 2.5475 g/micron
64.706 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 18.342 g/micron
465.89 g/mil
ISO 6383-2
Dart Drop Test 60.0 g
0.132 lb
F50; ISO 7765-1
Film Tensile Strength at Break, MD 45.0 MPa
6530 psi
ISO 527-3
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
1% Secant Modulus, MD 250 MPa
36300 psi
ISO 527-3
1% Secant Modulus, TD 290 MPa
42100 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
Internal method
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 13 %
13 %
ISO 14782
Gloss 50 %
50 %
45°; ASTM D2457