Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 440 MPa @Strain 0.200 % |
63800 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 440 MPa @Strain 1.00 % |
63800 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4762 High Temperature Ferritic Stainless Steel Highest chromium content-most resistant to reducing sulphurous gases. Susceptible to 475°C embrittlement and s-phase forms during long exposures in the range 600-800°C.Applications: Mostly used i.. |
|||
Tensile Strength, Yield | >= 440 MPa @Strain 1.00 % |
>= 63800 psi @Strain 1.00 % |
|
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24 Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me.. |
|||
Tensile Strength, Yield | >= 440 MPa @Strain 1.00 % |
>= 63800 psi @Strain 1.00 % |
|
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54 Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl.. |
|||
Tensile Strength, Yield | >= 440 MPa @Strain 0.200 %, Temperature 300 °C |
>= 63800 psi @Strain 0.200 %, Temperature 572 °F |
|
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | >= 440 MPa @Strain 0.200 %, Thickness 50.0 - 60.0 mm |
>= 63800 psi @Strain 0.200 %, Thickness 1.97 - 2.36 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Tensile Strength, Yield | >= 440 MPa @Strain 0.200 %, Thickness 150 - 240 mm |
>= 63800 psi @Strain 0.200 %, Thickness 5.91 - 9.45 in |
Tempers T651 / T652 |
Constellium Certal® SPC Aluminum Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man.. |
|||
Tensile Strength, Yield | >= 440 MPa @Diameter 63.0 mm |
>= 63800 psi @Diameter 2.48 in |
Re. Core strength in hardened condition. |
Assab Steels 7210M Machinery Steel ASSAB 7210M is an alloyed case hardening steel with high core strength.Applications: ASSAB 7210M is used for applications requiring a hard, wear resistant surface and a tough core, such as transmiss.. |