Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 340 MPa @Strain 0.200 % |
49300 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Yield | 340 MPa @Strain 0.200 % |
49300 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 340 MPa @Strain 1.00 % |
49300 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 340 MPa @Strain 1.00 % |
49300 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | 340 MPa @Strain 0.200 % |
49300 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4724 High Temperature Ferritic Stainless Steel Truly stainless high temperature grade with 13% chromium. Not critical in terms of embrittlement.Applications: Mostly used in high temperature applications with sulphurous atmospheres and/or low te.. |
|||
Tensile Strength, Yield | 340 MPa @Strain 1.00 % |
49300 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | >= 340 MPa @Strain 0.200 %, Thickness 152.4 - 203.2 mm |
>= 49300 psi @Strain 0.200 %, Thickness 6.000 - 8.000 in |
Tempers T651 / T652 |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength, Yield | 340 MPa @Strain 0.200 %, Thickness 254 - 305 mm |
49300 psi @Strain 0.200 %, Thickness 10.0 - 12.0 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength, Yield | >= 340 MPa @Strain 0.200 %, Thickness 450 - 700 mm |
>= 49300 psi @Strain 0.200 %, Thickness 17.7 - 27.6 in |
long-transverse direction |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Tensile Strength, Yield | >= 340 MPa @Strain 0.200 %, Thickness 450 - 700 mm |
>= 49300 psi @Strain 0.200 %, Thickness 17.7 - 27.6 in |
Temper T652 |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
Tensile Strength, Yield | >= 340 MPa @Strain 0.200 %, Thickness 15.0 - 35.0 mm |
>= 49300 psi @Strain 0.200 %, Thickness 0.591 - 1.38 in |
Temper T651 |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |
|||
Tensile Strength, Yield | >= 340 MPa @Strain 0.200 %, Thickness 35.0 - 60.0 mm |
>= 49300 psi @Strain 0.200 %, Thickness 1.38 - 2.36 in |
Temper T651 |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |
|||
Tensile Strength, Yield | 340 MPa @Temperature 260 °C |
49300 psi @Temperature 500 °F |
|
Crucible Steel XM-19 Stainless Steel Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio.. |