Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 300 MPa @Strain 0.200 %, Temperature 250 °C |
43500 psi @Strain 0.200 %, Temperature 482 °F |
EN min.; EN 10002-5 |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 % |
43500 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 %, Temperature -196 °C |
43500 psi @Strain 0.200 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 %, Temperature -196 °C |
43500 psi @Strain 0.200 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 % |
43500 psi @Strain 0.200 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 1.00 %, Temperature 100 °C |
43500 psi @Strain 1.00 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 % |
43500 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 % |
43500 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 % |
43500 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4529 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 % |
43500 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | >= 300 MPa @Temperature 20.0 °C |
>= 43500 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Tensile Strength, Yield | 300 MPa @Temperature 700.0 °C |
43500 psi @Temperature 1292 °F |
|
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki.. |
|||
Tensile Strength, Yield | >= 300 MPa @Strain 0.200 % |
>= 43500 psi @Strain 0.200 % |
|
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42 Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0... |
|||
Tensile Strength, Yield | 300 - 360 MPa @Strain 0.200 % |
43500 - 52200 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 300 BH High-strength Steel High-strength SteelComments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is ap.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 %, Temperature 100 °C |
43500 psi @Strain 0.200 %, Temperature 212 °F |
|
Magnesium Elektron Elektron® 675 Magnesium Wrought Alloy High strength wrought Mg alloy used for high performance components, including at elevated temperature. Excellent corrosion resistance and easily machined. Can be extruded, forged and hot formed. .. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 %, Temperature 200 °C |
43500 psi @Strain 0.200 %, Temperature 392 °F |
|
Magnesium Elektron Elektron® 675 Magnesium Wrought Alloy High strength wrought Mg alloy used for high performance components, including at elevated temperature. Excellent corrosion resistance and easily machined. Can be extruded, forged and hot formed. .. |
|||
Tensile Strength, Yield | 300 MPa @Strain 0.200 %, Thickness 4.00 - 8.00 mm |
43500 psi @Strain 0.200 %, Thickness 0.157 - 0.315 in |
Typical Strength; Standard EN 485-2 |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength, Yield | 300 MPa @Temperature 538 °C |
43500 psi @Temperature 1000 °F |
|
Crucible Steel XM-19 Stainless Steel Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio.. |
|||
Tensile Strength, Yield | 300 - 450 MPa @Thickness >=3.17 mm |
43500 - 65300 psi @Thickness >=0.125 in |
transverse |
American Utility Metals 3CR12® Stainless Steel 3CR12 is a weldable ferritic stainless steel, specifically designed for aggressive material handling applications. It is intended to provide the benefits of traditional stainless steel, such as stre.. |
|||
Tensile Strength, Yield | 300 MPa @Strain 1.00 % |
43500 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 904L High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |