American Utility Metals 3CR12® Stainless Steel

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer American Utility Metals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Utility Metals 3CR12® Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3CR12 is a weldable ferritic stainless steel, specifically designed for aggressive material handling applications. It is intended to provide the benefits of traditional stainless steel, such as strength, corrosion and abrasion resistance, durability and low maintenance. But it is also able to provide additional benefits such as good weldability and formability, making it capable of fabrication by conventional techniques.Because 3CR12 does not depend upon expensive alloying elements like Nickel and Molybdenum, it has maintained a consistently low cost advantage compared to other corrosion resisting materials. It also offers the option to reduce costs through eliminating protective treatments and corrosion allowances. In service, utility stainless steel goes on to generate savings in maintenance, improved productivity and longer service life. It is proven to offer lower life cycle costs than traditional materials where corrosion or abrasion affect service conditions.
Mechanical Properties Metric English Comments
Hardness, Brinell <= 220

@Thickness <=12.7 mm
<= 220

@Thickness <=0.500 in
<= 250

@Thickness >=12.7 mm
<= 250

@Thickness >=0.500 in
Tensile Strength >= 455 MPa
>= 66000 psi
transverse
Tensile Strength, Yield 280 - 450 MPa

@Thickness <=3.17 mm
40600 - 65300 psi

@Thickness <=0.125 in
transverse
300 - 450 MPa

@Thickness >=3.17 mm
43500 - 65300 psi

@Thickness >=0.125 in
transverse
Elongation at Break >= 18 %

@Thickness <=4.50 mm
>= 18 %

@Thickness <=0.177 in
transverse
>= 20 %

@Thickness >=4.50 mm
>= 20 %

@Thickness >=0.177 in
transverse
Charpy Impact >= 33.9 J

@Thickness >=3.17 mm
>= 25.0 ft-lb

@Thickness >=0.125 in
transverse
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 10.5 - 12.5 %
10.5 - 12.5 %
Iron, Fe 82.9 - 89.5 %
82.9 - 89.5 %
Remainder
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni <= 1.5 %
<= 1.5 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %