Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP KONDUIT OTF2AXXP PPS (Asia Pacific) LNP* Konduit* OTF2AXXP is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Thermal Carbon Fiber. Added features of this material include: Thermally Conductive, Electrically C.. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF) LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC LNP LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing 20% Milled Glass, 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific) LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66 LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | unlubricated thrust washer machine @ 10 fpm and 250 psi |
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | unlubricated thrust washer machine @ 10 fpm and 250 psi |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | unlubricated thrust washer machine @ 10 fpm and 250 psi |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | 40psi, 50ft/min; tested in accordance with LNP WI-0687 |
LNP Konduit® OTF-202-10 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically Conductive, Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; h.. |
|||
K (wear) Factor | 8.06 - 342 x 10-8 mm³/N-M | 4.00 - 170 x 10-10 in³-min/ft-lb-hr | Average value: 105 x 10<sup>-8</sup> mm³/N-M Grade Count:13 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
K (wear) Factor | 8.06 x 10-8 mm³/N-M | 4.00 x 10-10 in³-min/ft-lb-hr | 40psi, 50ft/min; tested in accordance with LNP WI-0687 |
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
K (wear) Factor | 8.06 - 500 x 10-8 mm³/N-M | 4.00 - 248 x 10-10 in³-min/ft-lb-hr | Average value: 203 x 10<sup>-8</sup> mm³/N-M Grade Count:12 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |