Mechanical Properties Metric English Comments
K (wear) Factor 6.04 - 894 x 10-8 mm³/N-M
3.00 - 444 x 10-10 in³-min/ft-lb-hr
Average value: 137 x 10<sup>-8</sup> mm³/N-M Grade Count:19
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP IFL36L PA6.12
LNP* LUBRICOMP* IFL36L is a compound based on Nylon 6/12 containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Low Extractable, Wear Resistant.
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am..
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As..
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66
LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66
LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant.
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66
LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant.
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 (Asia Pacific)
LNP* Lubricomp* RP004 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A..
K (wear) Factor 6.04 x 10-8 mm³/N-M
3.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66
LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
Copyright © lookpolymers.com All Rights Reserved