Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP OCL36XXP PPS - Linear (Europe-Africa-Middle East) LNP* LUBRICOMP* OCL36XXP is a compound based on PPS- Linear resin containing PTFE, Carbon Fiber. Added features include : Internally Lubricated, Electrically Conductive . |
|||
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su.. |
|||
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | |
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
K (wear) Factor | 38.3 x 10-8 mm³/N-M | 19.0 x 10-10 in³-min/ft-lb-hr | 40psi, 50ft/min; tested in accordance with LNP WI-0687 |
LNP Lubricomp® OCL-4036 Polyphenylene Sulfide, Carbon Fiber Reinforcement, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |