Mechanical Properties Metric English Comments
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP KONDUIT OTF2AXXP PPS (Asia Pacific)
LNP* Konduit* OTF2AXXP is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Thermal Carbon Fiber. Added features of this material include: Thermally Conductive, Electrically C..
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF)
LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC
LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC
LNP LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing 20% Milled Glass, 10% PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10
LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66
LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific)
LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66
LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT
LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES
LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
unlubricated thrust washer machine @ 10 fpm and 250 psi
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
unlubricated thrust washer machine @ 10 fpm and 250 psi
Cast Nylons Nycast® Nyloil® Lubricated Nylon
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
unlubricated thrust washer machine @ 10 fpm and 250 psi
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Konduit® OTF-202-10 Polyphenylene Sulfide, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically Conductive, Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; h..
K (wear) Factor 8.06 - 342 x 10-8 mm³/N-M
4.00 - 170 x 10-10 in³-min/ft-lb-hr
Average value: 105 x 10<sup>-8</sup> mm³/N-M Grade Count:13
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
K (wear) Factor 8.06 - 500 x 10-8 mm³/N-M
4.00 - 248 x 10-10 in³-min/ft-lb-hr
Average value: 203 x 10<sup>-8</sup> mm³/N-M Grade Count:12
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Copyright © lookpolymers.com All Rights Reserved