Mechanical Properties Metric English Comments
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
ASTM G77
Greene Tweed Arlon® 1330 PEEK
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES (Europe-Africa-Middle East)
LNP* Lubricomp* JX91198 is a compound based on Polyethersulfone resin containing Carbon Fiber, Proprietary Lubricant.
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UL002S PPA
LNP* LUBRICOMP* UL002S is a compound based on Polyphthalamide resin containing 10% PTFE. Added features of this grade include: Heat Stabilized, Wear Resistant.
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT
LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant.
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA
LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® PA6/6 CF33 ML2 BK 33% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 33% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceAp..
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66
LNP* THERMOCOMP* RC006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific)
LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t..
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 (Asia Pacific)
LNP* Thermocomp* RC006 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66
LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod
Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coe..
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM)
Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep..