Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
11.9 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
11.9 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRETECH Halogen-free Engineering Thermoplastics Halogen-free PRETECH engineering thermoplastics enable environmentally friendly and cost efficient V-0 product solutions with excellent mechanical and electrical properties. PRETECH combines high th.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AR is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ares colour effects. The colour package may effect performance.This data was supplie.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC810FE PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810FE is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ferrite colour effects. The colour package may effect performance.This data was supp.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC810SK is suitable for those applications that require sparkl.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 206 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 595CP Refrigeration and Extrusion Grade Lustran® ABS 595CP is refrigeration and extrusion grade, resistant to cyclopentane, and has high impact strength. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 970 Lustran® ABS 970 has high impact strength and good paintability. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1A |
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXLAC 320 Acrylonitrile Butadiene Styrene Saxalac 320 is a high impact resistant, easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.I.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXLAC 320U Acrylonitrile Butadiene Styrene Saxalac 320U is an UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66 Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL IH PA 6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 41 Nylon 66, Conditioned Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, Conditioned Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |