Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas re.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 22.8 °C |
6.20 ft-lb/in² @Temperature 73.0 °F |
ISO 180/1A |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -20.0 °C |
6.19 ft-lb/in² @Temperature -4.00 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 377 Plating, Injection Molding Grade |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -20.0 °C |
6.19 ft-lb/in² @Temperature -4.00 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 450 Injection Molding Grade Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1A |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -10.0 °C |
6.19 ft-lb/in² @Temperature 14.0 °F |
ISO 180 |
Dow T702-12N Polypropylene Impact Copolymer Resin Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR35 NL HS PA6.6, 35% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical HG-174 ABS, High Gloss, Super High Flow Information Provided by LG Chem |