Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | ISO 180 |
Solvay Engineered Polymers SEQUEL® 2300 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2300 engineered polyolefin is designed for large mold-in-color automotive interior applications that require high stiffness and dimensional stability over a broad temperature r.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | |
Lushan PA66+30%+10%AR-1A Nylon Toughener/PA Impact Modifier Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Europe-Africa-Middle East) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 180/1A |
SYNTHOS Forsan® 548 Acrylonitrile Butadiene Styrene (ABS) Easy flow, glossy, impact resistant.Applications: General purposeVarious technical parts, household appliances, hobby and office equipment, etc.Synthos was formerly known as Kaucuk. All information .. |
|||
Izod Impact, Notched (ISO) | >= 24.0 kJ/m² | >= 11.4 ft-lb/in² | |
Sibur ABS 2020-31M Molding Grade ABS Plastic With high thermal and light resistance for automobile building, stable to atmospheric conditions in thermal and electric ageing, contacting with food products, as well as with compounding with PC. |
|||
Izod Impact, Notched (ISO) | >= 24.0 kJ/m² | >= 11.4 ft-lb/in² | |
Sibur ABS 2020-32 Molding Grade ABS Plastic Thermal, light and atmospheric resistant with high fluidity for technical articles and parts of automobile building. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 180/1A |
SYNTHOS Krasten® FB28 High Impact Polystyrene And Polyethylene Blend Polymer blend HIPS/PE. High toughness, very good tensile properties and environmental stress cracking resistance. Processed mainly by extrusion and thermoforming. Production of sheets and films, tec.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 LNP* VERTON* RX89047 is a compound based on Nylon 66 resin containing Proprietary Fillers. Added feature of this grade is: Structural. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Europe-Africa-Middle East) LNP* Verton* RX89047 is a compound based on Nylon 66 resin. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-726 ABS Electro-plating |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature -50.0 °C |
11.4 ft-lb/in² @Temperature -58.0 °F |
|
Dow LDPE 779I Low Density Polyethylene DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps.. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl B2 V50 Nylon 6, 50% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl B2 ZV 50 Nylon 6, 50% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 24.0 - 69.4 kJ/m² @Temperature -50.0 - -50.0 °C |
11.4 - 33.0 ft-lb/in² @Temperature -58.0 - -58.0 °F |
Average value: 40.5 kJ/m² Grade Count:10 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |