Lushan PA66+30%+10%AR-1A Nylon Toughener/PA Impact Modifier

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyolefin
Manufacturer Lushan
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lushan PA66+30%+10%AR-1A Nylon Toughener/PA Impact Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener/PA impact modifier Lushan series has good response compatibility, elastomer dispersed in PA matrix rapidly to form the fine dispersed elastomer phase and the combined closely two-phase interface structure. Consequently, thereby Nylon thoughener/PA impact modifier Lushan series can be used for enhancing the toughness of nylon, and improving the impact resistant of the finished articles.Nylon Toughener Usage:1. As impact modifier for toughening Nylon products like PA6, PA66, etc. To improve the impact resistance, lower water absorption of nylon products:2. As compatibilizer for PA/PE, PA/PP alloy.Information provided by Lushan
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
Flexural Strength 175 MPa
25400 psi
Izod Impact, Notched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²