Polymer Property : Izod Impact, Notched (ISO) = 80.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
63.5*12.7*3.2; ISO 180/4A
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
Izod Impact, Notched (ISO) 80.0 - 90.0 kJ/m²
38.1 - 42.8 ft-lb/in²
Average value: 82.5 kJ/m² Grade Count:4
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® 22 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® 22 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® 24 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® 25 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® 27 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® 27 U Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® F 22 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® F 23 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® F 25 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® FC 22 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® FC 22 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® FC 23 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® FC 25 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® MX 1071 FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® MX 2021 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® F 23 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® FC 23 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® MX 2015 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® MX 2042 FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® A 221 PA66, DRY
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
Izod Impact, Notched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180
Styrolution Terblend® N NM-21 XP ABS+PA (Conditioned)
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin
Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL..
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Thickness >=5.00 mm
38.1 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac..
Izod Impact, Notched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/4A
Chi Mei Wonderlite® PC-110L Polycarbonate - UV Stabilized
Head Lamp
Izod Impact, Notched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/4A
Chi Mei Wonderlite® PC-110U Polycarbonate - UV Stabilized
UV Stabilized
Izod Impact, Notched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/4A
Chi Mei Wonderlite® PC-110N Polycarbonate - Flame Retardant
Opaque
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NB50 BK001 IH PA6, impact modified, black, extrusion grade
Information provided by Eurotec®
Izod Impact, Notched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Mitsubishi Xantar® 27 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Copyright © lookpolymers.com All Rights Reserved